前言:美标H型钢W21x57使用规范美标H型钢:一直以来,该厂中型线H350规格产品采用275规格坯料轧制,但在轧制过程中轧制速度往往大于炼
美标H型钢W21x57使用规范美标H型钢:一直以来,该厂中型线H350规格产品采用275规格坯料轧制,但在轧制过程中轧制速度往往大于炼钢工序的坯料下线速度,导致工序生产速度不匹配,制约了生产效率的提升。同时,炼钢工序生产240坯料时,型钢生产线的轧制速度比坯料生产速度慢,导致大量坯料落地、积压,降低了坯料热装效率,增加了生产成本。针对这一问题,该厂进行立项攻关,积极探索实施240坯料轧制H350规格产品的新工艺,通过对坯料加热温度、轧制道次、轧机孔型等进行系统优化,实现了试验成功。
美标H型钢尺寸表:
美标H型钢W4*13 W100*100*19.3 A36/A992/A572GR50
美标H型钢W5*16 W130*130*23.8 A36/A992/A572GR50
美标H型钢W5*19 W130*130*28.1 A36/A992/A572GR50
美标H型钢W6*9 W150*W100*13.5 A36/A992/A572GR50
美标H型钢W6*12 W150*W100*18 A36/A992/A572GR50
美标H型钢W6*16 W150*W100*24 A36/A992/A572GR50
美标H型钢W6*15 W150*150*22.5 A36/A992/A572GR50
美标H型钢W6*20 W150*150*29.8 A36/A992/A572GR50
美标H型钢W6*25 W150*150*37.1 A36/A992/A572GR50
美标H型钢W8*10 W200*100*15 A36/A992/A572GR50
美标H型钢W8*13 W200*100*19.3 A36/A992/A572GR50
美标H型钢W8*15 W200*100*22.5 A36/A992/A572GR50
美标H型钢W8*14 W200*135*21.4 A36/A992/A572GR50
美标H型钢W8**18 W200*135*26.6 A36/A992/A572GR50
美标H型钢W8*21 W200*135*31.3 A36/A992/A572GR50
美标H型钢W8*24 W200*165*35.9 A36/A992/A572GR50
美标H型钢W8*28 W200*165*41.7 A36/A992/A572GR50
美标H型钢W8*31 W200*200*46.1 A36/A992/A572GR50
美标H型钢W8*35 W200*200*52 A36/A992/A572GR50
美标H型钢型号表:
美标H型钢W8*40 W200*200*59 A36/A992/A572GR50
美标H型钢W8*48 W200*200*71 A36/A992/A572GR50
美标H型钢W8*58 W200*200*86 A36/A992/A572GR50
美标H型钢W8*67 W200*200*100 A36/A992/A572GR50
美标H型钢W10*12 W250*100*17.9 A36/A992/A572GR50
美标H型钢W10*15 W250*100*22.3 A36/A992/A572GR50
美标H型钢W10*19 W250*100*28.4 A36/A992/A572GR50
美标H型钢W10*22 W250*145*32.7 A36/A992/A572GR50
美标H型钢W10*26 W250*145*38.5 A36/A992/A572GR50
美标H型钢W10*30 W250*145*44.8 A36/A992/A572GR50
美标H型钢W10*33 W250*200*49.1 A36/A992/A572GR50
美标H型钢W10*39 W250*200*58 A36/A992/A572GR50
美标H型钢W10*45 W250*200*67 A36/A992/A572GR50
美标H型钢W10*49 W250*250*73 A36/A992/A572GR50
美标H型钢W10*54 W250*250*80 A36/A992/A572GR50
美标H型钢W10*60 W250*250*89 A36/A992/A572GR50
美标H型钢W10*68 W250*250*101 A36/A992/A572GR50
美标H型钢W10*77 W250*250*115 A36/A992/A572GR50
美标H型钢W10*88 W250*250*131 A36/A992/A572GR50
美标H型钢W10*100 W250*250*149 A36/A992/A572GR50
美标H型钢W10*112 W250*250*167 A36/A992/A572GR50
美标H型钢W12*14 W310*100*21 A36/A992/A572GR50
美标H型钢W12*16 W310*100*23.8 A36/A992/A572GR50
美标H型钢W12*19 W310*100*28.3 A36/A992/A572GR50
美标H型钢W12*22 W310*100*32.7 A36/A992/A572GR50
美标H型钢W12*26 W310*165*38.7 A36/A992/A572GR50
美标H型钢W12*30 W310*165*44.5 A36/A992/A572GR50
美标H型钢W12*35 W310*165*52 A36/A992/A572GR50
美标H型钢W12*40 W310*200*60 A36/A992/A572GR50
美标H型钢W12*45 W310*200*67 A36/A992/A572GR50
美标H型钢W12*50 W310*200*74 A36/A992/A572GR50
美标H型钢HEM理重表:
美标H型钢W12*53 W310*250*79 A36/A992/A572GR50
美标H型钢W12*58 W310*250*86 A36/A992/A572GR50
美标H型钢W12*65 W310*310*97 A36/A992/A572GR50
美标H型钢W12*72 W310*310*107 A36/A992/A572GR50
美标H型钢W12*79 W310*310*117 A36/A992/A572GR50
美标H型钢W12*87 W310*310*129 A36/A992/A572GR50
美标H型钢W12*96 W310*310*143 A36/A992/A572GR50
美标H型钢W12*106 W310*310*158 A36/A992/A572GR50
美标H型钢W12*120 W310*310*179 A36/A992/A572GR50
美标H型钢W12*136 W310*310*202 A36/A992/A572GR50
美标H型钢W12*152 W310*310*226 A36/A992/A572GR50
美标H型钢W12*170 W310*310*253 A36/A992/A572GR50
美标H型钢W12*190 W310*310*283 A36/A992/A572GR50
美标H型钢W14*22 W360*130*32.9 A36/A992/A572GR50
美标H型钢W14*26 W360*130*39 A36/A992/A572GR50
美标H型钢W14*30 W360*170*44.6 A36/A992/A572GR50
美标H型钢W14*34 W360*170*51 A36/A992/A572GR50
美标H型钢W14*38 W360*170*58 A36/A992/A572GR50
美标H型钢W14*43 W360*200*64 A36/A992/A572GR50
美标H型钢W14*48 W360*200*72 A36/A992/A572GR50
美标H型钢W14*53 W360*200*79 A36/A992/A572GR50
美标H型钢W14*61 W360*250*91 A36/A992/A572GR50
美标H型钢W14*68 W360*250*101 A36/A992/A572GR50
美标H型钢W14*74 W360*250*110 A36/A992/A572GR50
美标H型钢W14*82 W360*250*122 A36/A992/A572GR50
美标H型钢W14*90 W360*370*134 A36/A992/A572GR50
美标H型钢W14*99 W360*370*147 A36/A992/A572GR50
美标H型钢W14*109 W360*370*162 A36/A992/A572GR50
美标H型钢W14*120 W360*370*179 A36/A992/A572GR50
美标H型钢W14*132 W360*370*196 A36/A992/A572GR50
美标H型钢W14*145 W360*410*216 A36/A992/A572GR50
美标型钢:去应力退火去应力退火是将工件加热到Ac1以下的适当温度,保温一定时间后逐渐缓慢冷却的工艺方法。其目的是为了去除由于机械加工、变形加工、铸造、锻造、热处理以及焊接后等产生的残余应力。去应力退火工艺曲线见图1-3。不同的工件去应力退火工艺参数见表C。去应力退火的温度,一般应比最后一次回火温度低2~3℃,以免降低硬度及力学性能。对薄壁工件、易变形的焊接件,退火温度应低于下限。低温时效用于工件的半加工之后(如粗加工或次精加工之后),一般采用较低的温度。